Complete technical data sheet with print conditions, material properties, and performance specifications.
| Manufacturer | Eryone | |
| Product Name | Hyper-Speed ASA | |
| Filament Type | ASA | |
| Finish | Standard |
| Nozzle Temperature | 230-260 °C | |
| Bed Temperature | 75-90 °C | |
| Print Speed | 30-200 mm/s | |
| Build Surface Materials | Glass, PEI, Spring Steel Plate |
| Diameter | 1.75 mm ±0.03 | |
| Density | 1.05 g/cm³ | ASTM D792 (ISO 1183, GB/T1033) |
| Vicat Softening Temperature | 106 °C | ASTM D1525 (ISO 306, GB/T1633) |
| Heat Distortion Temperature | 82 °C | ASTM D648, 1.8MPa |
| Melt Index | 7 g/10 min | 220°C, 10kg |
| Tensile Strength (XY) | 34.8 MPa | GB/T1040.4, 50mm/min |
| Tensile Strength (Z) | 19 MPa | GB/T1843, 50mm/min |
| Elastic Modulus (XY) | 1345.3 MPa | GB/T1040.1-2006, 50mm/min |
| Elastic Modulus (Z) | 1233.5 MPa | GB/T1040.1-2006, 50mm/min |
| Elongation at Break (XY) | 1.9 % | GB/T1040.4, 50mm/min |
| Elongation at Break (Z) | 1.7 % | GB/T1040.4, 50mm/min |
| Bending Strength | 52.7 MPa | GB/T9341, 2mm/min |
| Bending Modulus | 1884.5 MPa | GB/T9341, 2mm/min |
| Charpy Impact Strength | 30.5 kJ/m² | GB/T1843, 2.75J |
| Technical Data Sheet | View Data Sheet(Version 1.0) |